仿威图机柜买回来,很多人第一眼只看板厚和喷漆。真正决定它后期会不会门关不严、并柜错缝、重载下沉的,是里面那圈型材。市面上叫“仿威图”的柜子不少,但骨架做法差一档,用两年就现原形。
When buying a replica Weitu cabinet, many people only see thick boards and spray paint at first glance. The true determinant of whether the doors will not close tightly, the cabinets will be staggered, and heavy loads will sink in the later stage is the circle of profiles inside. There are many cabinets called "imitation Weitu" on the market, but the skeleton construction is one level worse, and it only takes two years to show its original shape.
先分清两件事:德系原版威图常用的是十六折型材,国内多数仿威图走的是九折型材路线。九折不是简单把钢板折九道玩花样,而是每一折都承担一个功能——外沿挂门铰链、内腔走强弱电槽、侧边留并柜孔、底部固定底座。折数少一道,某个受力点就悬空。
First, let's distinguish two things: the original German version of Weitu commonly uses 16 fold profiles, while most domestic imitations of Weitu follow the 9 fold profile route. Nine fold folding is not simply playing tricks by folding steel plates nine times, but each fold serves a function - hanging door hinges on the outer edge, strong and weak electrical slots in the inner cavity, leaving cabinet holes on the side, and fixing the base at the bottom. If one fold is missing, a certain point of force will be suspended.

现场验收别听销售说“我们也是九折”,拿卡尺和角尺自己量三处:
On site inspection, don't listen to the salesperson saying 'we also offer a 10% discount'. Take a caliper and angle ruler and measure three places yourself:
单折边长与回弹
Single fold edge length and rebound
九折型材每道折边长度应一致,回弹角越小越好。用角尺靠外立面,缝隙能塞进 0.5mm 塞尺就偏软,重载门板挂上去会慢慢外张。
The length of each folded edge of the nine fold profile should be consistent, and the smaller the rebound angle, the better. Using an angle ruler against the exterior, if the gap can be filled with a 0.5mm feeler gauge, it will be too soft, and when a heavy load door panel is hung on it, it will slowly expand outward.
并柜孔位共面度
Coplanarity of parallel cabinet holes
两台柜并起来,用直尺贴前立柱,前后错位超过 1mm,门缝就会一边宽一边窄。九折型材如果折模磨损,孔位会累计偏移,三台以上并柜非常明显。
When two cabinets are put together and a ruler is used to stick the front pillar, if the front and rear displacement exceeds 1mm, the door gap will be wider on one side and narrower on the other. If the folding mold of the nine fold profile is worn, the hole position will accumulate offset, especially when three or more units are combined.
内部安装梁能否前后无级调
Can the internal installation beam be infinitely adjustable back and forth
真九折型材的内腔是带长条滑道的,安装梁螺丝能在槽里前后滑、任意位置锁紧。如果只能按固定孔距装,那叫“冲孔方管”,不叫九折。
The inner cavity of the true nine fold profile is equipped with a long sliding track, and the installation beam screws can slide back and forth in the groove and lock at any position. If it can only be installed according to a fixed hole spacing, it is called "punched square tube", not "nine fold".
再顺手看两个细节:
Take a closer look at two details:
角连接器:九折型材交接处应该用锌合金压铸角块+自攻钉,不是焊死。焊死的柜子运输一颠就变形,且没法现场改尺寸;
Corner connector: The junction of the nine fold profile should be made of zinc alloy die cast corner blocks and self tapping screws, not welded. The welded cabinet deforms easily during transportation and cannot be resized on site;
密封条槽:门板四周发泡条要嵌在型材预留槽里,不是拿胶粘在板边。粘的用半年就脱,槽嵌的压紧回弹一直在。
Sealing strip groove: The foam strip around the door panel should be embedded in the reserved groove of the profile, not glued to the edge of the board. The adhesive peeled off after half a year, and the groove was tightly pressed and bounced back all the time.
板厚 1.5mm 的柜体看着比 2.0mm 薄,但九折型材做对了,整体刚度反而比“厚板+方管骨架”稳。反过来,板再厚、型材是折四道凑数的,装完变频器一通电,门就合不严。
The cabinet with a thickness of 1.5mm looks thinner than 2.0mm, but the nine fold profile is done correctly, and the overall stiffness is actually more stable than the "thick plate+square tube skeleton". On the other hand, no matter how thick the board or profile is, it needs to be folded four times to make up the number. Once the inverter is installed and powered on, the door won't close tightly.
下次到货抽检,别只拍外观照。随机抽一台拆侧板,卡尺量折边、直尺靠并柜面、螺丝刀试安装梁滑动——这三下比看质保书管用。
Don't just take appearance photos for the next arrival inspection. Randomly select a side panel, use a caliper to measure the folded edge, use a ruler to align with the cabinet surface, and use a screwdriver to test the installation of the beam sliding - these three tests are more effective than checking the warranty certificate.